Additive Manufacturing Processes
Metal Powder Production and Powder Size and Shape Distribution
-
Published:2020
Abstract
This article provides an overview of the general methods of metal powder production. It details the primary methods for particle sizing used in additive manufacturing: sieving, laser diffraction and scattering, and digital image analysis. Methods of interpreting and understanding particle size distribution (PSD) data are presented, with an emphasis on the differences between count- and volume-based PSDs. The article then outlines practices for both qualitative and quantitative assessment of particle morphology.
Sign in
ASM members
Member Sign InZack Snow, Metal Powder Production and Powder Size and Shape Distribution, Additive Manufacturing Processes, Vol 24, ASM Handbook, Edited By David L. Bourell, William Frazier, Howard Kuhn, Mohsen Seifi, ASM International, 2020, p 167–171, https://doi.org/10.31399/asm.hb.v24.a0006567
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.