Appendix 11: Continuous Cooling Diagrams of Selected Steels Available to Purchase
-
Published:2008
Page range:
601 - 627
Abstract
This appendix is a collection of selected continuous cooling transformation diagrams for carbon steels; Mn steels; Mn-Mo, Mn-Ce, Mn-Ni-Mo, and Mn-Ni-CrMo steels; silicon steels; nickel steels; Ni-Cr-Mo steels; and chromium steels.
You do not currently have access to this chapter.
Citation
Continuous Cooling Diagrams of Selected Steels, Failure Analysis of Heat Treated Steel Components, Edited By Lauralice de C.F. Canale, Rafael A. Mesquita, George E. Totten, ASM International, 2008, p 601–627, https://doi.org/10.31399/asm.tb.fahtsc.t51130601
Download citation file:
Related Book Content
The History of Engineering Alloy Steels
The History of Metals in America
Isothermal Diagrams of Selected Steels
Failure Analysis of Heat Treated Steel Components
Heat Treatment
Metals Fabrication Understanding the Basics
Magnetically Soft Materials
Metals Handbook Desk Edition (2nd Edition)
Physical Properties of Carbon and Low-Alloy Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Internal Cracks in Cast Steel With 9% Ni for Cryogenic Applications
Handbook of Case Histories in Failure Analysis
Classification and Designation of Carbon and Low-Alloy Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Hardenability of Carbon and Alloy Steels
Metals Handbook Desk Edition (2nd Edition)
Physical Properties of Carbon and Low-Alloy Steels
Failure Analysis of Heat Treated Steel Components
Flux Cored Arc Welding
Welding Fundamentals and Processes