Steel heated in contact with air at temperatures in the tempering range takes on various temper colors due to the formation of a thin oxide film. This appendix provides information on the cause and source of oxidation of steel and time-temperature effect on SAE 1035 steel. In addition, figures that show temper colors after heating 1035 steel in circulating air are presented.
You do not currently have access to this chapter.
Citation
Temper Colors for Steels, Failure Analysis of Heat Treated Steel Components, Edited By Lauralice de C.F. Canale, Rafael A. Mesquita, George E. Totten, ASM International, 2008, p 539–540, https://doi.org/10.31399/asm.tb.fahtsc.t51130539
Download citation file:
Related Book Content
Electric Arc Furnace Melting
Casting
Automotive Exhaust System Corrosion
Corrosion: Environments and Industries
AISI-SAE System of Designations for Steels
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Cross-Reference to Steels
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Introduction—Purpose of Text, Microstructure and Analysis, Steel Definitions, and Specifications
Steels: Processing, Structure, and Performance (Second Edition)
Steel as a Material
Metallography of Steels Interpretation of Structure and the Effects of Processing
Failure of a Nylon Filtration Unit
ASM Failure Analysis Case Histories: Failure Modes and Mechanisms
Steel Cross Reference to AISI/SAE Designations
Heat Treating of Irons and Steels
Introduction
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
History and Primary Steel Processing
Steels: Processing, Structure, and Performance (Second Edition)