Abstract
This appendix is a collection of tables listing examples of published hardness conversion equations, approximate Rockwell B and C hardness conversion numbers for nonaustenitic steels, and equivalent hardness numbers for Brinell hardness numbers and Vickers (diamond pyramid) hardness numbers for steel.
You do not currently have access to this chapter.
Citation
Steel Hardness Conversions, Failure Analysis of Heat Treated Steel Components, Edited By Lauralice de C.F. Canale, Rafael A. Mesquita, George E. Totten, ASM International, 2008, p 529–535, https://doi.org/10.31399/asm.tb.fahtsc.t51130529
Download citation file:
Sept. 30 – Oct. 4 | Cleveland, Ohio
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2024 & IFHTSE World Congress!
Related Book Content
Introduction—Purpose of Text, Microstructure and Analysis, Steel Definitions, and Specifications
Steels: Processing, Structure, and Performance (Second Edition)
Steel as a Material
Metallography of Steels Interpretation of Structure and the Effects of Processing
AISI-SAE System of Designations for Steels
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Cross-Reference to Steels
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Steel Cross Reference to AISI/SAE Designations
Heat Treating of Irons and Steels
History and Primary Steel Processing
Steels: Processing, Structure, and Performance (Second Edition)
Introduction
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Steel Hardness Conversions
Metallurgy for the Non-Metallurgist (Second Edition)
Decarburization of Steels
Practical Heat Treating (Second Edition)
Glossary of Terms: Surface Engineering
Surface Engineering