Failure Analysis of Powder Metal Steel Components Available to Purchase
-
Published:2008
Abstract
This chapter reviews failure aspects of structural ferrous powder metallurgy (PM) parts, which form the bulk of the PM industry. The focus is on conventional PM technology of parts in the density range of 6 to 7.2 g/cc. The chapter briefly introduces the processing steps that are essential to understanding failure analysis of PM parts. This is followed by a section on case hardening of PM parts. The methods used for analyzing the failures are then discussed. Some case studies are given that illustrate different failures and the methods of prevention of these failures.
S. Ashok, Sundar Sriram, Failure Analysis of Powder Metal Steel Components, Failure Analysis of Heat Treated Steel Components, Edited By Lauralice de C.F. Canale, Rafael A. Mesquita, George E. Totten, ASM International, 2008, p 395–415, https://doi.org/10.31399/asm.tb.fahtsc.t51130395