Failure Analysis of Heat Treated Steel Components
General Aspects of Failure Analysis
-
Published:2008
Abstract
This chapter briefly outlines some of the basic aspects of failure analysis, describing some of the basic steps and major concerns in conducting a failure analysis. A brief review of failure types from fracture, distortion, wear-assisted failure, and environmentally assisted failure (corrosion) is also provided.
Sign in
ASM members
Member Sign InWaldek Wladimir Bose-Filho, José Ricardo Tarpani, Marcelo Tadeu Milan, General Aspects of Failure Analysis, Failure Analysis of Heat Treated Steel Components, Edited By Lauralice de C.F. Canale, Rafael A. Mesquita, George E. Totten, ASM International, 2008, p 111–132, https://doi.org/10.31399/asm.tb.fahtsc.t51130111