Failure Analysis of Heat Treated Steel Components
Failure Analysis of Heat Treated Steel Components discusses failures and how to determine their root cause. The book focuses on steel failures that arise during thermal processing, such as forging, casting, heat treatment, and welding. The metallurgy of the failure identification is also examined. Topics covered include component design, mechanisms of failures in heat treated steel parts, general aspects of failure analysis, failures in steel forging, failures from the casting process, sources of failures in carburized and carbonitrided components, fatigue fracture of nitride layers, steel heat treatment failures due to quenching, steel failures due to tempering and isothermal heat treatment, failure analysis in tool steels, case studies of steel component failures in aerospace applications, failure analysis of powder metal steel components, induction hardening, and failure analysis of steel welds. For information on the print version, ISBN 978-0-87170-868-7, follow this link.
Download citation file:
Table of Contents
-
Component DesignByMario Solari;Mario SolariCTI Consultores de Tecnología e Ingeniería SRLSearch for other works by this author on:Pablo BilmesPablo BilmesUniversidad Nacional de La PlataSearch for other works by this author on:
-
Overview of the Mechanisms of Failure in Heat Treated Steel ComponentsByScott MacKenzieScott MacKenzieHoughton International, Inc.Search for other works by this author on:
-
Mechanisms and Causes of Failures in Heat Treated Steel PartsByDebbie AliyaDebbie AliyaAliya Analytical, Inc.Search for other works by this author on:
-
General Aspects of Failure AnalysisByWaldek Wladimir Bose-Filho;Waldek Wladimir Bose-FilhoUniversidade de São PauloSearch for other works by this author on:José Ricardo Tarpani;José Ricardo TarpaniUniversidade de São PauloSearch for other works by this author on:Marcelo Tadeu MilanMarcelo Tadeu MilanInstituto de Materiais Tecnológicos do Brasil Ltda.Search for other works by this author on:
-
Failure in Steel ForgingByMd. Maniruzzaman;Md. ManiruzzamanWorcester Polytechnic InstituteSearch for other works by this author on:Richard D. Sisson, Jr.;Richard D. Sisson, Jr.Worcester Polytechnic InstituteSearch for other works by this author on:
-
Failures from the Casting ProcessByOmar Maluf;Omar MalufInstituto de Materiais Tecnológicos do Brasil Ltda.Search for other works by this author on:Luciana Sgarbi Rossino;Luciana Sgarbi RossinoInstituto de Materiais Tecnológicos do Brasil Ltda.Search for other works by this author on:Camilo Bento Carletti;Camilo Bento CarlettiUniversidade Federal de São CarlosSearch for other works by this author on:Celso Roberto Ribeiro;Celso Roberto RibeiroUniversidade Federal de São CarlosSearch for other works by this author on:Clever Ricardo Chinaglia;Clever Ricardo ChinagliaUniversidade Federal de São CarlosSearch for other works by this author on:José Eduardo MayJosé Eduardo MayUniversidade Federal de São CarlosSearch for other works by this author on:
-
Sources of Failures in Carburized and Carbonitrided ComponentsByMałgorzata Przyłęcka;Małgorzata PrzyłęckaPoznan University of TechnologySearch for other works by this author on:Wojciech Gęstwa;Wojciech GęstwaPoznan University of TechnologySearch for other works by this author on:Lauralice C.F. Canale;Lauralice C.F. CanaleUniversity of São PauloSearch for other works by this author on:G.E. TottenG.E. TottenAssociação Instituto Internacional de Ciência and Portland State UniversitySearch for other works by this author on:
-
Fatigue Fracture of Nitrided LayersByAleksander NakoniecznyAleksander NakoniecznyInstitute of Precision MechanicsSearch for other works by this author on:
-
Steel Heat Treatment Failures due to QuenchingByG.E. TottenG.E. TottenAssociação Instituto Internacional de Ciência and Portland State UniversitySearch for other works by this author on:
-
Steel Failures due to Tempering and Isothermal Heat TreatmentByJan Vatavuk;Jan VatavukUniversidade Presbiteriana MackenzieSearch for other works by this author on:L.C.F. CanaleL.C.F. CanaleUniversidade de São Paulo USPSearch for other works by this author on:
-
Failure Analysis in Tool SteelsByRafael Agnelli Mesquita;Rafael Agnelli MesquitaVillares MetalsSearch for other works by this author on:Celso Antonio BarbosaCelso Antonio BarbosaVillares MetalsSearch for other works by this author on:
-
Case Studies of Steel Component Failures in Aerospace ApplicationsByScott MacKenzieScott MacKenzieHoughton International, Inc.Search for other works by this author on:
-
Failure Analysis of Powder Metal Steel ComponentsBySundar SriramSundar SriramSundram Fasteners Ltd.Search for other works by this author on:
-
Induction HardeningByJanez GrumJanez GrumUniversity of LjubljanaSearch for other works by this author on:
-
Failure Analysis of Steel WeldsBy