This chapter discusses the application of high-pressure cold spray to the automotive industry field, with special attention to three applications: additive manufacturing, fabrication methods, and protective coatings. Various studies on the automotive application of cold spray are reviewed. The background and purpose of each application are presented and practical cases are discussed.
You do not currently have access to this chapter.
Citation
C. Lee, J. Kim, Cold Spray Applications in the Automotive Industry, High Pressure Cold Spray: Principles and Applications, Edited By Charles M. Kay, J. Karthikeyan, ASM International, 2016, p 209–226, https://doi.org/10.31399/asm.tb.hpcspa.t54460209
Download citation file:
Related Book Content
Powder Production Techniques for High-Pressure Cold Spray
High Pressure Cold Spray Principles and Applications
Modeling and Simulation of Cold Spray
High Pressure Cold Spray Principles and Applications
Cold Spray Applications in Repair and Refurbishment for the Aerospace, Oil and Gas, and Power-Generation Industries
High Pressure Cold Spray Principles and Applications
Introduction
Advanced-High Strength Steels Science, Technology, and Applications
Applications of Advanced High-Strength Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Introduction to Advanced High-Strength Steels
Advanced High-Strength Steels: Science, Technology, and Applications, Second Edition
Alkyd Resins
Protective Organic Coatings
Armament Corrosion
Corrosion: Environments and Industries
Elemental Chemistry Introduction
Protective Organic Coatings
Failure of Gas Turbine Last- Stage Bucket
ASM Failure Analysis Case Histories: Power Generating Equipment