Induction Heating and Heat Treatment
Methods, Tools, and Software for Physical Process Analysis and Design
-
Published:2014
Abstract
Designing of induction heating, or, generally electro technological installations, requires mathematical modeling for solving problems related to various physical phenomena, including electromagnetic (EM), thermal, mechanical, fluidic, and metallurgical fields. This article focuses on the solution of Maxwell's equations (MEs) and provides some basic information regarding the heat transfer and fluid equations, because these physical phenomena usually are strongly coupled to magnetic and electric fields. The solutions are usually obtained by using specific numerical methods such as finite-element method, finite difference method, boundary-element method or volume-integral method, and direct-solution method. The article also discusses the typical structure of commercial codes...
Sign in
ASM members
Member Sign InMichele Forzan, Methods, Tools, and Software for Physical Process Analysis and Design, Induction Heating and Heat Treatment, Vol 4C, ASM Handbook, Edited By Valery Rudnev, George E. Totten, ASM International, 2014, p 243–260, https://doi.org/10.31399/asm.hb.v04c.a0005876
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!