Components, Design, and Operation of Vacuum Induction Crucible Furnaces
-
Published:2014
Abstract
This article discusses the principle, coil design, types and operation of a vacuum induction furnace. It describes the operation parameters that should be considered during the functioning of the induction furnace.
Egbert Baake, Components, Design, and Operation of Vacuum Induction Crucible Furnaces, Induction Heating and Heat Treatment, Vol 4C, ASM Handbook, Edited By Valery Rudnev, George E. Totten, ASM International, 2014, p 462–466, https://doi.org/10.31399/asm.hb.v04c.a0005900