Electromagnetic Problem Solutions
-
Published:2014
Abstract
Electromagnetic problem solutions are based on the macroscopic theory of the continuous model for the electromagnetic field (EMF). It is described by a system of integral or partial differential equations for five vector quantities, namely, electric field strength, electric flux density, current density, magnetic field strength, and magnetic flux density. This article describes the behavior of the EMF by Maxwell's equations in integral or differential forms. It discusses the definition of potentials; methods of mathematical modeling; boundary conditions; and energy, power density, and electromagnetic forces.
Jerzy Barglik, Dagmara Dołęga, Electromagnetic Problem Solutions, Induction Heating and Heat Treatment, Vol 4C, ASM Handbook, Edited By Valery Rudnev, George E. Totten, ASM International, 2014, p 261–265, https://doi.org/10.31399/asm.hb.v04c.a0005877
Download citation file:
Data Ecosystem
The ASM Data Ecosystem arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.