Abstract
Induction hardening is a prominent method in the gear manufacturing industry due to its ability of selectively hardening portions of a gear such as the flanks, roots, and/or tips of teeth with desired hardness, wearing resistance, and contact fatigue strength without affecting the metallurgy of the core. This article provides an overview of gear technology and materials selection. It describes different gear-hardening patterns, namely, tooth-by-tooth hardening, tip-by-tip hardening, gap-by-gap hardening, spin hardening, single-frequency gear hardening, dual-frequency gear hardening, simultaneous dual-frequency gear hardening, and through heating for surface hardening. It provides information on the different inspection methods based on the American Gear Manufacturers Association, revealing metallurgical data, hardness, and dimensions of gears. In addition, the article presents a comparative study on the mechanical properties of contour-hardened and carburized gears. It concludes by describing typical failures of induction-hardened steels and the corresponding prevention methods.
Valery Rudnev, John Storm, Induction Hardening of Gears and Gear-Like Components, Induction Heating and Heat Treatment, Vol 4C, ASM Handbook, Edited By Valery Rudnev, George E. Totten, ASM International, 2014, p 187–210, https://doi.org/10.31399/asm.hb.v04c.a0005867
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!