Melting of Glasses and Oxides
-
Published:2014
Abstract
This article provides an overview of the models of two induction heating devices, namely, induction crucible furnace (ICF) and induction furnace with slits, or segmented and water-cooled induction furnace with cold crucible (IFCC). These devices are used for melting with skull formation of low-conductivity materials such as glasses and oxides. The article presents the governing equations and boundary conditions for ICF and IFCC modeling. It includes a discussion on three electromagnetic field models in IFCC, namely, two-dimensional (2-D), quasi-three-dimensional, and three-dimensional (3-D) models. The article provides information on the simulation of skull formation in IFCC, and elucidates the transient axisymmetrical 2-D model and the transient 3-D model, including the primary results achieved for both glasses and skull formation.
Andris Jakovics, Sergejs Pavlovs, Melting of Glasses and Oxides, Induction Heating and Heat Treatment, Vol 4C, ASM Handbook, Edited By Valery Rudnev, George E. Totten, ASM International, 2014, p 535–547, https://doi.org/10.31399/asm.hb.v04c.a0005907
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.