Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)
Chapter 8: Stress-Corrosion Cracking of Aluminum Alloys[1]
Retired
-
Published:2017
Abstract
Aluminum is protected by a barrier oxide film that, if damaged, reforms immediately in most environments. Despite this inherent corrosion resistance, there are conditions where aluminum alloys, like many materials, are subject to the effects of stress-corrosion cracking (SCC). This chapter describes those conditions, focusing initially on the effects of alloying elements and temper on solution potential and how it compares to other metals. It then addresses the issue of intergranular corrosion and its role in SCC. It explains how factors such as stress loads, grain structure, and environment determine whether or not stress-corrosion cracking develops in a susceptible...
Sign in
ASM members
Member Sign InR.H. Jones, Stress-Corrosion Cracking of Aluminum Alloys, Stress-Corrosion Cracking: Materials Performance and Evaluation, 2nd ed., Edited By Russell H. Jones, ASM International, 2017, p 241–256, https://doi.org/10.31399/asm.tb.sccmpe2.t55090241
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.