ASM Handbook
Heat Treating of Nonferrous Alloys
Edited by
George E. Totten
George E. Totten
Portland State University
Search for other works by this author on:
ASM International
Volume
4E
ISBN electronic:
978-1-62708-169-6
Publication date:
2016
Abstract
This article presents a detailed discussion on typical thermal treatment practices for hardening of various aluminum casting alloys. These practices are solution treatment, quenching or cooling, preaging, and artificial aging at an elevated temperature. The aluminum casting alloys considered here are: Al-Cu and Al-Cu-Mg (2xx) alloys, Al-Zn-Mg (7xx) alloys, Al-Si-Mg alloys, Al-Si-Cu, and Al-Si-Cu-Mg alloys.
You do not currently have access to this chapter.
Citation
Geoffrey K. Sigworth, Heat Treatment of Aluminum Alloy Castings, Heat Treating of Nonferrous Alloys, Vol 4E, ASM Handbook, Edited By George E. Totten, ASM International, 2016, p 274–288, https://doi.org/10.31399/asm.hb.v04e.a0006264
Download citation file:
Related Book Content
Heat Treatment
Casting
Heat Treatment of Aluminum Alloy Castings
Aluminum Science and Technology
Heat Treatment Practices of Age-Hardenable Aluminum Alloys
Heat Treating of Nonferrous Alloys
Metallurgy of Heat Treatable Aluminum Alloys
Heat Treating of Nonferrous Alloys
Metallurgy of Heat Treatable Aluminum Alloys
Aluminum Science and Technology
Quenching of Aluminum Alloys
Aluminum Science and Technology
Annealing of Aluminum and Its Alloys
Heat Treating of Nonferrous Alloys
Heat Treatment of Aluminum Castings
Aluminum Alloy Castings Properties, Processes, and Applications
Modeling and Simulation of the Heat Treatment of Aluminum Alloys
Heat Treating of Nonferrous Alloys
Residual Stress in Heat Treatable Aluminum Alloys
Heat Treating of Nonferrous Alloys