Microelectronics Failure Analysis: Desk Reference (Seventh Edition)
Section 5: FIB Technique and Circuit Edit
-
Published:2019
Abstract
With the commercialization of heavier and lighter ion beams, adoption of focused ion beam (FIB) use for analysis of challenging regions of interest (ROI) has grown. In this chapter, the authors focus on highlighting commercially available and complementary FIB technologies and their implementation challenges and application trends.
Abstract
Circuit edit has been instrumental to the development of focused ion beam (FIB) systems. FIB tools for advanced circuit edit play a major role in the validation of design and manufacture. This chapter begins with an overview of value, role, and unique capabilities of FIB circuit edit tools for first silicon debug. The etching capabilities of circuit edit FIB tools are then discussed, providing information on chemistry assisted etching in silicon oxides and low-k dielectrics. The chapter also discusses the requirements and procedures involved in edit operation: high aspect ratio milling, endpointing, and cutting copper. It then provides an introduction to FIB metal/conductor deposition and FIB dielectric deposition. Edit design rules that can facilitate prototype production from first silicon are also provided. The chapter concludes with a discussion on future trends in circuit edit technology.
Sign in
ASM members
Member Sign InFIB Technique and Circuit Edit, Microelectronics Failure Analysis: Desk Reference, 7th ed., Edited By Tejinder Gandhi, ASM International, 2019
Download citation file: