The 14-cm diam main hoist shaft of a mobile shovel was found to have multiple crack indications when ultrasonically inspected in the field. A crack around the entire circumference at the change in section was revealed by magnetic-particle inspection of the shaft. The crack was found to coincide with the junction of the fillet and the smaller diam at this change in section. A slight step in the continuity of the fillet and some machining marks were noted at this junction. A fine crack extending 2.5 mm from the surface and originating at the machining marks was revealed by...