A flat spring for the main landing gear of a light aircraft failed after safe execution of a hard landing. The spring material was identified by chemical analysis to be 6150 steel. The fracture was found to have occurred near the end of the spring that was inserted through a support member about 25 mm thick and attached to the fuselage by a single bolt. Brinelling (plastic flow and indentation due to excessive localized contact pressure) was observed on the upper surface of the spring where the forward and rear edges of the spring contacted the support member. It...