Porcelain enamel is a fusion bonded glass coating that resists chemical and abrasive attack, provides thermal and electrical insulation, and improves aesthetic qualities. It is used on cast iron as well as steel and aluminum alloys. This article provides a review of the porcelain enameling process, the composition of frits, and the preparation of coating substrates. It also provides information on chemical, mechanical, and electrical properties and sheds light on process consistency and quality control.