This article presents an approach to manage the uncertainty present in materials design. It describes inductive and deductive approaches to deal with uncertainty. The article focuses on providing an understanding of the opportunities for managing uncertainty and the decisions that influence the accuracy of the results. A design of experiments (DOE) represents a sequence of experiments to be performed, expressed in terms of factors set at specified levels. The article discusses the two types of DOEs: the full factorial design and the fractional factorial design. It explains the factors to be considered when selecting a procedure for propagating uncertainty. The article lists the categories of the popular types of uncertainty propagation methods, including simulation-based methods, local expansion methods, and numerical integration-based methods.