This article provides a review of fatigue test methodologies and an overview of general fatigue behavior, fatigue crack initiation and fatigue crack propagation of advanced engineering plastics. It also describes the factors affecting fatigue performance of polymers and concludes with information on fractography, a useful tool in failure analysis.