This article provides an overview of two major classes of bearings: rolling bearings and sliding, or plain, bearings. It reviews the experimental data resulted from testing of rolling and sliding bearing materials with illustration. The article presents a table that summarizes rolling contact fatigue test methods that ASTM published in STP 771. It also describes the role of lubrication in the bearings.