Corrosion Monitoring for Industrial Processes
-
Published:2003
Abstract
This article describes the criteria for selecting a corrosion-monitoring method used in industrial plants. It provides a detailed discussion on the design, advantages, and disadvantages of plant corrosion-testing program. The basic types of racks used to support and insulate the coupons are also discussed. The analysis of electrical-resistance probes, sentry holes, side-stream loop, electrochemical noise, hydrogen-probe, and process streams are used to monitor and estimate corrosion rates. The corrosion rates can also be estimated by ultrasonic thickness measurements, polarization-resistance measurements, corrosion potential measurements, and alternating current impedance measurements. Corrosion monitoring strategies, such as locations, data analysis, redundancy, and other issues, are discussed. The article concludes with information on the interpretation and reporting of corrosion testing.
Sign in
ASM members
Member Sign InSheldon W. Dean, Corrosion Monitoring for Industrial Processes, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 533–541, https://doi.org/10.31399/asm.hb.v13a.a0003659
Download citation file:
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.