This article reviews the general characteristics of copper and copper alloys and explains how these characteristics affect the behavior of strip in different types of forming operations. These forming operations include blanking, piercing, bending, drawing and stretch forming, spinning, rubber-pad forming, and contour roll forming. Specialized forming operations such as hydraulic forming, embossing and swaging, and high-velocity metal forming are also reviewed. The article discusses the forming of smaller and larger parts from copper and copper alloy strips, as well as their property requirements and applications.