Stress-corrosion cracking (SCC) is a cracking phenomenon that occurs in susceptible alloys, and is caused by the conjoint action of tensile stress and the presence of a specific corrosive environment. This article provides an overview of the anodic dissolution mechanisms and cathodic mechanisms for SCC. It discusses the materials, environmental, and mechanical factors that control hydrogen embrittlement and SCC behavior of different engineering materials with emphasis on carbon and low-alloy steels, high-strength steels, stainless steels, nickel-base alloys, aluminum alloys, and titanium alloys.