Abstract

This article discusses the factors influencing cast iron machining and selection of cutting fluid and cutting tool materials. It presents a comparison of machinability of different types of cast iron, namely, gray cast iron, ductile cast iron, and malleable cast iron. In addition, the article provides an overview of different methods used in the machining of cast iron, namely, turning, boring, broaching, planing and shaping, drilling, reaming, counterboring and spotfacing, tapping, milling, grinding, and honing and lapping. Nominal speeds and feeds for the machining of cast iron with single-point and box tools, ceramic tools, high-speed steel, and carbide tools are also tabulated.