This article provides accessible information on the thermodynamic properties of liquid aluminum-base and copper-base alloys with the help of phase diagrams. It contains tables that compile thermodynamic data in the form of activities, activity coefficients, partial molar thermal properties, and integral molar properties for selected aluminum-base and copper-base alloys.