Abstract

Density allows for conversion of uniform corrosion rates from units of weight (or mass) loss per unit area per time to thickness per unit time. This article contains a table that lists density of metals and alloys. These include aluminum, copper, iron, stainless steels, magnesium, lead, and their alloys.