Surface Engineering
Volume 5 provides application-oriented information on surface engineering for a wide range of materials, topographies, and length scales. It addresses surface cleaning and preparation; coating, plating, and deposition processes; testing and characterization; and proper setup and use of equipment and instrumentation. It also includes a wealth of tabular data and graphs, describing process parameters, solution compositions, operating conditions, and finishing techniques for various irons and steels; aluminum, copper, magnesium, nickel, titanium, and zirconium alloys; and high-performance ceramics, polymers, and composites. In addition, the volume examines application-specific cases such as cutting tools, corrosive and abrasive environments, thin films, and extreme temperatures. It also covers dip, barrier, and chemical conversion coating processes, surface modification, electroplating, diffusion coating, chemical and physical vapor deposition, and other controlled-atmosphere processes. For information on the print version of Volume 5, ISBN: 978-0-87170-384-2, follow this link.
Download citation file:
Table of Contents
-
Surface CleaningByRobert E. LuetjeRobert E. LuetjeKolene CorporationSearch for other works by this author on:
-
Classification and Selection of Cleaning ProcessesByDavid B. ChalkDavid B. ChalkRevising authorTexo CorporationSearch for other works by this author on:
-
Alkaline CleaningByGerald J. CormierGerald J. CormierRevising authorParker+Amchem, Henkel CorporationSearch for other works by this author on:
-
Solvent Cold Cleaning and Vapor DegreasingByVicki L. Rupp;Vicki L. RuppRevising authorDow Chemical USASearch for other works by this author on:Ken SurprenantKen SurprenantRevising authorDow Chemical USASearch for other works by this author on:
-
Emulsion CleaningBySteven M. NourieSteven M. NourieRevising authorAmerican Metal Wash Inc.Search for other works by this author on:
-
Molten Salt Bath CleaningByJames C. MalloyJames C. MalloyKolene CorporationSearch for other works by this author on:
-
Ultrasonic CleaningByJeff HancockJeff HancockBlue Wave UltrasonicsSearch for other works by this author on:
-
Acid CleaningByKenneth J. HaciasKenneth J. HaciasRevising authorParker + Amchem, Henkel CorporationSearch for other works by this author on:
-
Mechanical Cleaning SystemsByTed KostilnikTed KostilnikRevising authorWheelabrator CorporationSearch for other works by this author on:
-
-
Finishing Methods
-
Classification and Selection of Finishing ProcessesByK. SubramanianK. SubramanianWorld Grinding Technology Center, Norton CompanySearch for other works by this author on:
-
Finishing Methods Using Defined Cutting EdgesByV.C. Venkatesh;V.C. VenkateshGintic Institute of Manufacturing Technology, Nanyang Technological University,SingaporeSearch for other works by this author on:S. EnomotoS. EnomotoGintic Institute of Manufacturing Technology, Nanyang Technological University,SingaporeSearch for other works by this author on:
-
Finishing Methods Using Multipoint or Random Cutting EdgesByK. SubramanianK. SubramanianWorld Grinding Technology Center, Norton CompanySearch for other works by this author on:
-
Nonabrasive Finishing MethodsByK.P. Rajurkar;K.P. RajurkarNontraditional Manufacturing Research Center, University of Nebraska-LincolnSearch for other works by this author on:Jerzy Kozak;Jerzy KozakNontraditional Manufacturing Research Center, University of Nebraska-LincolnSearch for other works by this author on:Arindam ChatterjeeArindam ChatterjeeNontraditional Manufacturing Research Center, University of Nebraska-LincolnSearch for other works by this author on:
-
Mass FinishingByEdward H. TulinskiEdward H. TulinskiRevising authorHarper Surface Finishing Systems, Inc.Search for other works by this author on:
-
Shot PeeningByTed KostilnikTed KostilnikRevising authorWheelabrator CorporationSearch for other works by this author on:
-
Topography of SurfacesByR.K. MortonR.K. MortonRank Taylor Hobson Inc.Search for other works by this author on:
-
Thermal Aspects of Surface Finishing ProcessesBy
-
Selection, Application, and Disposal of Finishing FluidsByCynthia K. CordellCynthia K. CordellMaster Chemical CorporationSearch for other works by this author on:
-
Influence of Work Material Properties on Finishing MethodsByK. SubramanianK. SubramanianWorld Grinding Technology Center, Norton CompanySearch for other works by this author on:
-
-
Plating and ElectroplatingByMyron E. BrowningMyron E. BrowningMatrix Technologies, Inc.Search for other works by this author on:
-
Copper PlatingByL.M. Weisenberger;L.M. WeisenbergerRevising authorMacDermid, Inc.Search for other works by this author on:B.J. DurkinB.J. DurkinRevising authorMacDermid, Inc.Search for other works by this author on:
-
Industrial (Hard) Chromium PlatingByKenneth R. NewbyKenneth R. NewbyRevising authorAtotech USASearch for other works by this author on:
-
Decorative Chromium PlatingByJames H. Lindsay;James H. LindsayRevising authorGeneral MotorsSearch for other works by this author on:Donald L. SnyderDonald L. SnyderRevising authorAtotech USA Inc.Search for other works by this author on:
-
Nickel PlatingByGeorge A. Di BariGeorge A. Di BariRevising authorInternational Nickel Inc.Search for other works by this author on:
-
Iron PlatingBySue Troup-PackmanSue Troup-PackmanHughes Research LaboratoriesSearch for other works by this author on:
-
Cadmium PlatingByMilton F. Stevenson, Sr.Milton F. Stevenson, Sr.Revising authorAnoplate CorporationSearch for other works by this author on:
-
Zinc PlatingByA. SatoA. SatoRevising authorLea Ronal Inc.Search for other works by this author on:
-
Indium PlatingByAllen W. Grobin, Jr.Allen W. Grobin, Jr.Grobin Associates, Inc.Search for other works by this author on:
-
Tin PlatingByArthur J. KillmeyerArthur J. KillmeyerRevising authorTin Information Center of North AmericaSearch for other works by this author on:
-
Lead PlatingByGeorge B. RynneGeorge B. RynneRevising authorNovamax TechnologySearch for other works by this author on:
-
Silver PlatingByAlan BlairAlan BlairAT&T Bell LaboratoriesSearch for other works by this author on:
-
Platinum-Group Metals PlatingByCh.J. RaubCh.J. RaubForschungsinstitut für Edelmetalle und MetallchemieSearch for other works by this author on:
-
Tin Alloy PlatingByReginald K. Asher, Sr.Reginald K. Asher, Sr.Motorola Semiconductor Product SectorSearch for other works by this author on:
-
Zinc Alloy PlatingByNabil ZakiNabil ZakiFrederick Gumm Chemical Company, Inc.Search for other works by this author on:
-
Nickel Alloy PlatingByS. Alec WatsonS. Alec WatsonNickel Development InstituteSearch for other works by this author on:
-
Chromium Alloy PlatingByEric W. BroomanEric W. BroomanConcurrent Technologies CorporationSearch for other works by this author on:
-
Multiple-Layer Alloy PlatingByDaniel T. SchwartzDaniel T. SchwartzUniversity of WashingtonSearch for other works by this author on:
-
ElectroformingByMyron E. BrowningMyron E. BrowningMatrix TechnologiesSearch for other works by this author on:
-
Electroless Nickel PlatingByDonald W. BaudrandDonald W. BaudrandRevising authorMacDermid Inc.Search for other works by this author on:
-
Electroless Copper PlatingByCheryl A. DeckertCheryl A. DeckertShipley Company, Inc.Search for other works by this author on:
-
Electroless Alloy DepositionByPhillip D. StapletonPhillip D. StapletonStapleton TechnologiesSearch for other works by this author on:
-
-
Dip, Barrier, and Chemical Conversion CoatingsBy
-
Continuous Hot Dip CoatingsByHerbert E. TownsendHerbert E. TownsendBethlehem Steel CorporationSearch for other works by this author on:
-
Continuous Electrodeposited Coatings for Steel StripByStavros G. FountoulakisStavros G. FountoulakisBethlehem Steel CorporationSearch for other works by this author on:
-
Batch Hot Dip Galvanized CoatingsByDonald WetzelDonald WetzelRevising authorAmerican Galvanizers AssociationSearch for other works by this author on:
-
BabbittingByWilliam P. Bardet;William P. BardetPioneer Motor Bearing CompanySearch for other works by this author on:Donald J. WenglerDonald J. WenglerPioneer Motor Bearing CompanySearch for other works by this author on:
-
Chromate Conversion CoatingsByPatrick L. Hagans;Patrick L. HagansNaval Research LaboratorySearch for other works by this author on:Christina M. HaasChristina M. HaasHenkel CorporationSearch for other works by this author on:
-
Rust-Preventive CompoundsByHarry D. Ferrier, Jr.Harry D. Ferrier, Jr.Revising authorQuaker Chemical CorporationSearch for other works by this author on:
-
PaintingByJeffrey P. Gossner;Jeffrey P. GossnerRevising authorPreFinish Metals Inc.Search for other works by this author on:Kenneth B. TatorKenneth B. TatorRevising authorKTA-Tator, Inc.Search for other works by this author on:
-
Elastomeric Coatings for Automotive PlasticsBy
-
Ceramic Coatings and LiningsByWoodrow W. CarpenterWoodrow W. CarpenterRevising authorThe Ceramic Coating CompanySearch for other works by this author on:
-
AnodizingByMilton F. Stevenson, Jr.Milton F. Stevenson, Jr.Revising authorAnoplate CorporationSearch for other works by this author on:
-
Vacuum and Controlled-Atmosphere Coating and Surface Modification
-
Thermal Spray CoatingsByRobert C. Tucker, Jr.Robert C. Tucker, Jr.Praxair Surface Technologies, Inc.Search for other works by this author on:
-
Chemical Vapor Deposition of Semiconductor MaterialsByManijeh RazeghiManijeh RazeghiNorthwestern UniversitySearch for other works by this author on:
-
Plasma-Enhanced Chemical Vapor DepositionByRafael ReifRafael ReifMassachusetts Institute of TechnologySearch for other works by this author on:
-
Sputter DepositionByS.L. RohdeS.L. RohdeUniversity of Nebraska-LincolnSearch for other works by this author on:
-
Ion-Beam-Assisted DepositionByGraham K. Hubler;Graham K. HublerNaval Research LaboratorySearch for other works by this author on:James K. HirvonenJames K. HirvonenU.S. Army Research LaboratorySearch for other works by this author on:
-
Arc DepositionByDavid M. Sanders;David M. SandersLawrence Livermore National LaboratorySearch for other works by this author on:Joseph W. Glaser;Joseph W. GlaserLawrence Livermore National LaboratorySearch for other works by this author on:Steven FalabellaSteven FalabellaLawrence Livermore National LaboratorySearch for other works by this author on:
-
Ion ImplantationByJames K. Hirvonen;James K. HirvonenU.S. Army Research LaboratorySearch for other works by this author on:Bruce D. SartwellBruce D. SartwellU.S. Naval Research LaboratorySearch for other works by this author on:
-
Pulsed-Laser DepositionByJames S. HorwitzJames S. HorwitzNaval Research LaboratorySearch for other works by this author on:
-
-
Testing and Characterization of Coatings and Thin FilmsByGary E. McGuireGary E. McGuireMicroelectronics Center of North CarolinaSearch for other works by this author on:
-
Film Thickness Measurements Using Optical TechniquesByHarland G. TompkinsHarland G. TompkinsMotorola, Inc.Search for other works by this author on:
-
Corrosion Testing of CoatingsByHermann A. Jehn;Hermann A. JehnResearch Institute for Precious Metals and Metals ChemistrySearch for other works by this author on:Andreas ZielonkaAndreas ZielonkaResearch Institute for Precious Metals and Metals ChemistrySearch for other works by this author on:
-
Stress Determination for CoatingsByJ. Albert Sue;J. Albert SuePraxair Surface Technologies, Inc.Search for other works by this author on:Gary S. SchajerGary S. SchajerUniversity of British ColumbiaSearch for other works by this author on:
-
Testing of Stability and Thermal Properties of Thermal Barrier CoatingsByThomas A. Taylor;Thomas A. TaylorPraxair Surface Technologies, Inc.Search for other works by this author on:
-
Surface and Interface Analysis of Coatings and Thin FilmsByS. HofmannS. HofmannMax-Planck-Institut für Metallforschung, Institut für Werkstoffwissenschaft,Stuttgart,GermanySearch for other works by this author on:
-
-
Surface Engineering of Irons and Steels
-
Surface Engineering of Nonferrous MetalsByFrederick S. PettitFrederick S. PettitUniversity of PittsburghSearch for other works by this author on:
-
Surface Engineering of Heat-Resistant AlloysByF.S. PettitF.S. PettitRevising authorUniversity of PittsburghSearch for other works by this author on:
-
Surface Engineering of Magnesium AlloysByJames E. HillisJames E. HillisRevising authorDow Chemical CompanySearch for other works by this author on:
-
Surface Engineering of Titanium and Titanium AlloysByT. BellT. BellUniversity of Birmingham,U.K.Search for other works by this author on:
-
Surface Engineering of Zirconium and HafniumByR. Terrence WebsterR. Terrence WebsterRevising authorMetallurgical ConsultantSearch for other works by this author on:
-
Surface Engineering of Refractory Metals and AlloysByJohn A. Shields, Jr.John A. Shields, Jr.Revising authorClimax Specialty MetalsSearch for other works by this author on:
-
Surface Engineering of Nickel and Nickel AlloysByRussell C. BuckleyRussell C. BuckleyRevising authorNordam Propulsion Systems DivisionSearch for other works by this author on:
-
Surface Engineering of Zinc AlloysByThomas P. GroeneveldThomas P. GroeneveldRevising authorBattelle Columbus OperationsSearch for other works by this author on:
-
-
Surface Engineering of Selected Nonmetallic MaterialsByCharles A. ParkerCharles A. ParkerAlliedSignal, Inc.Search for other works by this author on:
-
Surface Engineering for Chemical ActivityByJennifer S. FeeleyJennifer S. FeeleyEngelhard CorporationSearch for other works by this author on:
-
Protective Coatings for Carbon-Carbon CompositesByJames R. Strife;James R. StrifeUnited Technologies Research CenterSearch for other works by this author on:
-
Plasma Surface Engineering of PlasticsByOm S. KolluriOm S. KolluriAIRCO Coating TechnologySearch for other works by this author on:
-
Environmental Protection IssuesByLuis D. TrupiaLuis D. TrupiaGrumman Aircraft SystemsSearch for other works by this author on:
-
Environmental Regulation of Surface EngineeringByDavid J. SmukowskiDavid J. SmukowskiBoeing Commercial Airplane GroupSearch for other works by this author on:
-
Cadmium Elimination in Surface EngineeringByMark W. IngleMark W. IngleCorrpro Companies, Ocean City Research CorporationSearch for other works by this author on:
-
Chromium Elimination in Surface EngineeringByElwin JangElwin JangUnited States Air Force, Sacramento Air Logistics CenterSearch for other works by this author on:
-
Vapor Degreasing AlternativesByTony L. Green;Tony L. GreenLockheed Aeronautical Systems CompanySearch for other works by this author on:Donald W. Benjamin;Donald W. BenjaminAlliedSignal AerospaceSearch for other works by this author on:
-
Compliant Organic CoatingsByThomas E. KearneyThomas E. KearneyCourtaulds AerospaceSearch for other works by this author on:
-
Compliant Wipe Solvent Cleaners[1]ByMark T. CarrollMark T. CarrollLockheed Fort Worth CompanySearch for other works by this author on:
-
-
Reference Information