The stress-strain curves in this data set are representative examples of the behavior of several cast alloys under tensile or compressive loads. The curves are arranged by alloy designation. Each figure cites the original source of the curve and provides pertinent background information as available. Compressive tangent modulus curves are presented for certain alloys. The effects of cyclic loading are given on several curves.