Abstract

This data set contains approximately 50 growth curves for a wide range of aluminum casting alloys at various temperatures. Growth curves are used to determine the dimensional changes that must be anticipated during service in applications where close dimensional tolerances are required. Hardness curves are provided for many of the alloys. The hardness values are from corresponding aging response studies in which measurements were made on individual lots considered representative of the respective alloys and tempers.