This chapter covers the tribological properties of different types of oil, greases, solid lubricants, and metalworking and traction fluids. It explains how lubricants are made, how they work, and how they are applied and tested. It also discusses the fundamentals of lubrication and friction control, the relationship between viscosity and breakaway friction, and the factors that affect load-carrying capacity and service life.