Abstract

This chapter describes a number of corrosion testing methods for sintered stainless steels, including immersion, salt spray, and electrochemical tests, ferric chloride and ferroxyl tests, and elevated-temperature oxidation resistance tests. It also provides corrosion resistance and performance data from various sources.