Abstract
Titanium castings are used in a wide range of aerospace, chemical process, marine, biomedical, and automotive applications. This chapter provides an overview of titanium casting and associated processes and how they compare with other manufacturing methods. It also discusses the role heat treating and its effect on the tensile properties of different titanium alloys.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Castings, Titanium: A Technical Guide, 2nd ed., By Matthew J. Donachie, Jr., ASM International, 2000, p 39–45, https://doi.org/10.31399/asm.tb.ttg2.t61120039
Download citation file:
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.
Related Topics
Related Book Content
Titanium Alloys
Lightweight Materials Understanding the Basics
Titanium and Its Alloys for Biomedical Implants
Materials for Medical Devices
Processing of Titanium and Titanium Alloys
Metals Handbook Desk Edition, 2nd Ed. (2nd Edition)
Foundry Practice for Nonferrous Alloys
Metals Handbook Desk Edition, 2nd Ed. (2nd Edition)
Casting
Metals Fabrication Understanding the Basics
Forging of Discontinuously Reinforced Aluminum Composites
Metalworking: Bulk Forming
Failures from the Casting Process
Failure Analysis of Heat Treated Steel Components
Aluminum Casting Applications
Aluminum Castings Engineering Guide
Process Selection Guidelines
Aluminum Castings Engineering Guide