This chapter discusses the various methods used to join titanium alloy assemblies, focusing on welding processes and procedures. It explains how welding alters the structure and properties of titanium and how it is influenced by composition, surface qualities, and other factors. It describes several welding processes, including arc welding, resistance welding, and friction stir welding, and addresses related issues such as welding defects, quality control, and stress relieving. The chapter also covers mechanical fastening techniques along with adhesive bonding and brazing.