Book Chapter
Chapter 18: Design and Certification Considerations
-
Published:2010
Abstract
This chapter discusses design and certification considerations, including materials and process selection, the building block approach to certification, design allowables, and design guidelines. It also includes information on damage tolerance and environmental sensitivity.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Design and Certification Considerations, Structural Composite Materials, By F.C. Campbell, ASM International, 2010, p 489–515, https://doi.org/10.31399/asm.tb.scm.t52870489
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.