Skip Nav Destination
Close
ASM INTERNATIONAL
View Catalog
>
ASM Technical Books
Structural Composite Materials
ASM International
ISBN electronic:
978-1-62708-314-0
Publication date:
2010
Book Chapter
Chapter 8: Adhesive Bonding
-
Published:2010
Abstract
This chapter explains how polymeric adhesives are applied to composite as well as metal parts, forming bonded structures. It describes surface preparation practices and techniques, epoxy selection and use, and bonding procedures.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Adhesive Bonding, Structural Composite Materials, By F.C. Campbell, ASM International, 2010, p 235–254, https://doi.org/10.31399/asm.tb.scm.t52870235
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.
Related Topics
Related Book Content
Medical Adhesives
Materials for Medical Devices
Adhesive Bonding
Aluminum Science and Technology
Joining of Organic-Matrix Composites
Welding, Brazing and Soldering
Adhesive Bonding and Mechanical Fasteners
Beryllium Chemistry and Processing
Introduction and Overview of Joining
Metals Handbook Desk Edition, 2nd Ed. (2nd Edition)
Joining and Assembly of Polymer-Matrix Composites
Engineered Materials Handbook Desk Edition
Joining and Assembly of Plastics
Engineered Materials Handbook Desk Edition
An Overview of Joining Processes
Welding Fundamentals and Processes
Safe Welding Practices
Welding Fundamentals and Processes
Design for Joining
Materials Selection and Design