This chapter discusses the use of thermoset and thermoplastic resins in polymer matrix composites. It begins by explaining how the two classes of polymer differ and how it impacts their use as matrix materials. It then goes on to describe the characteristics of polyester, vinyl ester, epoxy, bismaleimide, cyanate ester, polyimide, and phenolic resins and various toughening methods. The chapter also covers thermoplastic matrix materials and product forms and provides an introduction to the physiochemical tests used to characterize resins and cured laminates.

You do not currently have access to this chapter.
Don't already have an account? Register

Matrix Resin Systems, Structural Composite Materials, By F.C. Campbell, ASM International, 2010, p 63–100, https://doi.org/10.31399/asm.tb.scm.t52870063