Chapter 9: Decarburization and Defects
-
Published:2015
Abstract
This chapter explains how to recognize decarburization and related defects. It includes images showing how decarburization appears in various steels, discusses stock removal practices, and describes common defects and flaws such as quench cracks and where they are typically found.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Decarburization and Defects, Practical Induction Heat Treating, 2nd ed., By Richard E. Haimbaugh, ASM International, 2015, p 175–190, https://doi.org/10.31399/asm.tb.piht2.t55050175
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.