Book Chapter
Chapter 1: History of Metallurgy and Induction Heating
-
Published:2015
Abstract
This chapter provides a brief review of the scientific and technological developments leading to the widespread use of induction heat treating and its many applications in industry.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
History of Metallurgy and Induction Heating, Practical Induction Heat Treating, 2nd ed., By Richard E. Haimbaugh, ASM International, 2015, p 1–7, https://doi.org/10.31399/asm.tb.piht2.t55050001
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.