Sheet metal spinning is a forming technique that produces axially symmetric hollow bodies with nearly any contour. It is often used in combination with flow forming and shear spinning to manufacture a wide range of complex parts. This chapter describes the operating principles, stress states, and failure modes of each process along with typical applications and tooling requirements.