Any forming process that converts stored energy to plastic deformation in less than a few milliseconds is considered a high-velocity or impulse forming process. This chapter discusses the operating principles, equipment, and applications of the most common high-rate forming processes, including high-velocity hydroforming, high-velocity mechanical forming, and electromagnetic or energy-based forming.