This chapter provides a brief overview of nickel-iron-base, cobalt-base, and nickel-base superalloys, discussing their basic metallurgy and defining characteristics.

You do not currently have access to this chapter.
Don't already have an account? Register

Overview of Superalloys, Superalloys: Alloying and Performance, By Blaine Geddes, Hugo Leon, Xiao Huang, ASM International, 2010, p 9–15, https://doi.org/10.31399/asm.tb.sap.t53000009