Abstract

This chapter discusses corrosion prevention methods used with aluminum and its alloys. The methods range from relatively straightforward measures, such as proper handling and storage, to advanced early warning corrosion monitoring systems for military aircraft. The chapter summarizes the basic factors that influence design for corrosion resistance and discusses the use of conversion coatings, organic coatings, porcelain enameling, and electroplating. It also discusses corrosion monitoring methods used in chemical processing and refining industries.

You do not currently have access to this chapter.