Chapter 4: Intergranular and Exfoliation Corrosion
-
Published:1999
Abstract
This chapter describes the mechanisms, characteristics, and prevention of intergranular and exfoliation corrosion in various aluminum alloys. It discusses susceptible alloys and recommended tempers and presents several examples of exfoliation in aircraft components. It also explains how the two forms of corrosion are related to stress-corrosion cracking.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Intergranular and Exfoliation Corrosion, Corrosion of Aluminum and Aluminum Alloys, Edited By J.R. Davis, ASM International, 1999, p 63–74, https://doi.org/10.31399/asm.tb.caaa.t67870063
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.