This article provides an overview of common analytical tools used as part of the process of providing practical information regarding the causes of a coating problem or failure. The common analytical tools include Fourier transform infrared spectroscopy, differential scanning calorimetry, scanning electron microscopy-energy dispersive X-ray spectroscopy, chromatography, and electrochemical impedance spectroscopy. Test cabinets and standard test environments for laboratory analysis are reviewed. The article describes non-standard simulation testing and case studies of simulated environments for coating failure analysis.