High-Temperature Corrosion and Materials Applications
Chapter 17: Hydrogen Attack
-
Published:2007
Abstract
Carbon and low-alloy steels in high-temperature service are vulnerable to the effects of hydrogen attack, which include severe loss in tensile and rupture strengths as well as ductility. As the chapter explains, when steel is in contact with hydrogen molecules at elevated temperatures, hydrogen atoms can be absorbed at the surface and then diffuse into the metal. Hydrogen atoms in the metal then react with iron carbide forming methane gas which can accumulate at grain boundaries and other interfaces. The chapter describes two applications, one in coal-fired boilers, the other in petroleum refining, where hydrogen attack was observed. It documents the extent of the damage in each case and identifies the source of the hydrogen.
Sign in
ASM members
Member Sign InHydrogen Attack, High-Temperature Corrosion and Materials Applications, By George Y. Lai, ASM International, 2007, p 437–441, https://doi.org/10.31399/asm.tb.htcma.t52080437
Download citation file:
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.