Chapter 11: Oil-Fired Boilers and Furnaces
-
Published:2007
Abstract
Fireside corrosion can be a serious problem in oil-fired boilers and in refinery furnaces fired with low-grade fuels. This chapter provides an overview of fireside or oil-ash corrosion and the problems it can cause in utility power boilers and petrochemical refinery furnaces. It explains how oil-ash corrosion affects waterwalls, superheaters, and reheaters as well as metal tube supports and hangers.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Oil-Fired Boilers and Furnaces, High-Temperature Corrosion and Materials Applications, By George Y. Lai, ASM International, 2007, p 321–334, https://doi.org/10.31399/asm.tb.htcma.t52080321
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.