Chapter 2: Challenges in Materials Applications for High-Temperature Service
-
Published:2007
Abstract
This chapter explains how materials selection becomes much more difficult when designing for high-temperature corrosion environments. It also discusses the use of cladding and weld overlays to compensate for material deficiencies and prolong service life.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Challenges in Materials Applications for High-Temperature Service, High-Temperature Corrosion and Materials Applications, By George Y. Lai, ASM International, 2007, p 3–4, https://doi.org/10.31399/asm.tb.htcma.t52080003
Download citation file:
Close
ASM INTERNATIONAL
FALL / WINTER 2020 CATALOG
View the new, upcoming, and best-selling resources in ASM Handbooks, technical books, and databases in the Fall / Winter 2020 Catalog.