Fracture control can be defined as a concerted effort to maintain operating safety without catastrophic failure by fracture. It requires an understanding of how cracks affect structural integrity and strength and the time that a crack can grow before it exceeds permissible size. The chapter describes some of methods used to determine maximum permissible crack size and predict growth rates. It explains how the information can then be used to control fractures through periodic inspection, fail-safe features, mandated retirement, and proof testing. It presents a number of fracture control plans optimized for different circumstances, examines the damage tolerance requirements...